Replacement hydraulic ram rods for Kinshofer grab buckets can be manufactured in-house, machined, weld prepped and welded to new clevis ends, ready to build straight into a ram. Simply Welding manufactured a batch of new Kinshofer hydraulic ram rods. We made this batch in our workshop, from machining the threaded ends through to welding on the clevis ends.
We made new hydraulic ram rods for Kinshofer grab buckets in our workshop. Each rod was machined, weld prepped, preheated and welded to its clevis end, ready to be built into a ram.
The threaded end of each rod was machined first, so the rod was ready to take its piston.
The clevis end of each rod was then machined and prepared for welding, giving a clean, strong joint with the clevis.
Before welding, the rod end and clevis were preheated with a gas torch, and the temperature was checked with an infrared thermometer.
With the rod held upright in a rotating welding positioner, the clevis was MIG welded on, running the weld right round the joint in one continuous run.
A batch of finished ram rods with their clevis ends welded on, ready to be assembled into Kinshofer hydraulic rams.
Preheating the rod end and clevis before welding slows the cooling of the weld, which helps prevent cracking and gives a stronger joint. We check the temperature with an infrared thermometer before welding.
Holding the rod upright in a rotating welding positioner lets us run the weld right round the joint in one continuous run, giving a consistent, even weld all the way round.
Yes. We hold Kinshofer KM602 and KM622 ram parts in stock, so most Kinshofer ram repairs can be completed the same day.
Want to see more of what we do?
Case Studies | Gallery
Need a new ram rod or a Kinshofer ram repaired? Call 07747 682451 or send us some photos via WhatsApp.